Paint & Coatings
Pigments, resins and additives for paints, inks and coatings — opacity, colour consistency, tack control and surface performance.

What determines how well a coating covers?
Hiding power is almost entirely a pigment question, and in a white or light-coloured coating it is a titanium dioxide question. TiO₂ scatters light so strongly that a few percent in the dry film will hide the substrate completely, and no alternative white pigment approaches it at comparable cost.
Rutile grades are specified for durability and opacity; anatase gives a brighter, cooler white but is photocatalytically more active and will accelerate degradation of the binder around it in an exterior coating. For anything exposed outdoors, a properly surface-treated rutile grade is the correct specification.
Why does surface treatment matter in a coating?
More than in plastics, because the pigment sits in an organic binder exposed directly to weather. Alumina and silica treatments do two jobs: they improve dispersion and wetting in the millbase, and they passivate the particle surface so that ultraviolet energy absorbed by the pigment does not attack the binder.
The visible failure when this is wrong is chalking — a surface where the binder has degraded and loose pigment can be wiped off. A weathering-grade pigment carries heavier treatment and therefore slightly lower TiO₂ content, which is the grade doing exactly what it should.
What role do rosin derivatives play?
Rosin and its esters are long-established tackifying and film-forming resins. Gum rosin is the base material, while the modified esters are used where stability and compatibility matter more than raw tack.
Glycerol esters of rosin offer improved colour and thermal stability over unmodified rosin, with good compatibility across adhesive and coating systems. Pentaerythritol esters go further, with higher softening points and better oxidation resistance, which suits hot-melt adhesives and coatings facing higher service temperature. Typical applications span printing inks, adhesives, varnishes and road-marking paint.
How are deep colours and blacks achieved?
Carbon black provides tinting strength and jetness, and grade selection has a direct effect on the finished appearance. Finer particle sizes give higher jetness and a bluer undertone but are harder to disperse and raise millbase viscosity; coarser grades disperse more readily with a browner undertone. In exterior coatings carbon black also provides ultraviolet screening, protecting the binder beneath.
What protects a coating over its service life?
Binder degradation is the limiting factor for exterior durability. UV absorbers and hindered amine light stabilisers address it by complementary routes — absorbers intercept the radiation before it reaches the binder, HALS interrupt the radical cycle once it starts — and they are commonly used together in high-durability systems. Antioxidants protect against thermal oxidation during manufacture and storage.
Sourcing from Revona
Revona Chemicals supplies these raw materials from Istanbul, with technical and safety documentation and samples available on request. Tell our team the system, the substrate and the exposure, and we will work back to the grades that fit.