Elastomers and compounding additives for seals, hose, belting and moulded rubber goods — oil, weather, flame and temperature resistance by application.

Rubber

How do you choose between the common elastomers?

Elastomer selection is usually settled by whichever environment is most hostile, because no single rubber is good at everything and the trade-offs are well understood.

Oil and fuel contact points to nitrile rubber. Weather, ozone and ultraviolet exposure points to EPDM. A specification demanding oil, weather and flame resistance together points to chloroprene rubber, which is the only common elastomer that is respectable at all three. Revona Chemicals supplies all three, along with the additives that go with them.

What does acrylonitrile content change in NBR?

Almost everything that matters. The polar nitrile groups are what resist oil swell, and the more acrylonitrile in the chain, the better the oil resistance — but the same polarity stiffens the chain, so cold flexibility falls in step.

Low-ACN grades around 18–20% stay flexible to roughly −40 °C but swell noticeably in oil. High-ACN grades at 45–50% resist oil and fuel strongly but stiffen not far below freezing. Medium grades at 33–36% are the general-purpose range covering most seal and gasket work. The practical method is to start from whichever requirement is harsher and verify the other can still be met.

NBR's weakness is weather: its unsaturated butadiene segments are attacked by ozone, and an unprotected part cracks outdoors. Blending with PVC improves this substantially, which is why NBR/PVC blends are common for hose covers and cable jackets.

Why does EPDM dominate outdoor applications?

Because its main chain is saturated. Ozone attacks carbon–carbon double bonds, and EPDM confines its unsaturation to a small side-chain diene used only as a cure site. With nothing in the backbone to attack, it resists weather, ozone, UV and steam almost indefinitely — which is why it dominates roofing membrane, window and automotive weather seals.

Two compositional figures drive grade selection. Ethylene content, typically 45–75%, sets crystallinity: high-ethylene grades carry high filler and oil loadings with good shape retention in extrusion, while low-ethylene grades stay flexible in the cold and give better compression set. Diene content sets sulphur cure rate.

The cure system is a real decision. Peroxide curing gives markedly better compression set and heat resistance — essential for a seal that must keep sealing after years under load — while sulphur curing is more economical and gives better tensile and tear properties.

Where does chloroprene fit?

Chloroprene is cured through metal oxides rather than sulphur, usually zinc oxide with magnesium oxide, which also acts as an acid acceptor and improves scorch safety. Grade families differ by polymerisation modifier: sulphur-modified grades give building tack and tear strength for hose and belting construction, while mercaptan-modified grades offer better heat ageing and storage stability.

One practical point for a cold warehouse: chloroprene crystallises during prolonged cold storage and stiffens. The effect is reversible by warming before processing.

Which additives support rubber compounding?

Carbon black is the primary reinforcing filler, with grade and loading setting hardness, modulus and abrasion resistance. Chlorinated polyethylene serves both as a polymer for weather- and oil-resistant compounds and as a modifier. Where flame performance is specified, aluminium hydroxide and zinc borate provide halogen-free routes, and antimony trioxide serves as synergist in halogenated systems.

Sourcing from Revona

Technical and safety data sheets and samples are available on request. Describe the service environment and the tests the part must pass, and our team will work back to the elastomer and the compounding package.