EPDM has a fully saturated backbone, which is why it simply does not care about ozone, weather or UV — the properties that make it the standard for anything living outdoors.

  • CAS Number: 25038-36-2
EPDM Rubber

At a glance

Category Polymers
CAS Number 25038-36-2
Chemical name Ethylene propylene diene monomer rubber
Appearance Bales or pellets
Ethylene content Typically 45–75%; higher ethylene gives greater green strength and filler acceptance
Diene content Typically 2–10% ENB; controls cure rate with sulphur systems
Service temperature Typically −50 °C to +130 °C depending on compound and cure system
Curing Sulphur (via the diene) or peroxide for better heat and compression set
Typical applications Roofing membrane, window and automotive seals, hose, cable insulation, brake system parts
Packaging 25 kg bales on pallets
Documentation TDS and SDS on request
Supplied from Istanbul, Türkiye

Need this material?

Tell us the application, the specification and the volume you work with. Our team will come back with availability and the documentation you need.

Description

Why EPDM resists weather so well

Most synthetic rubbers carry double bonds along the main chain, and ozone attacks exactly those sites — which is why an unprotected nitrile or natural rubber part cracks outdoors. EPDM is built differently: its backbone is a saturated ethylene–propylene chain, with unsaturation confined to a small amount of diene hung off to the side purely so the material can be sulphur-cured.

With nothing for ozone to attack in the main chain, EPDM resists weather, ozone, UV and steam almost indefinitely, which is why it dominates applications where a rubber part must survive years of outdoor exposure.

Ethylene and diene content

Two compositional figures govern behaviour. Ethylene content, usually between 45% and 75%, determines how much crystallinity the polymer carries. High-ethylene grades have greater green strength, accept very high filler and oil loadings, and extrude with good shape retention — useful for dense profile and for highly extended compounds. Low-ethylene grades are amorphous, stay flexible at low temperature and give better compression set.

Diene content, typically 2% to 10% as ethylidene norbornene, sets the cure rate for sulphur systems. More diene means a faster, tighter cure, at a modest cost in heat ageing.

Sulphur or peroxide cure

Sulphur curing works through the diene, is economical and gives good mechanical properties. Peroxide curing cross-links the backbone directly, producing carbon–carbon bonds that survive heat far better and give markedly better compression set — essential for a seal that must stay sealing after years under load at temperature. Peroxide-cured compounds are more expensive and need care in formulating, since many common ingredients interfere with peroxide cure.

Where EPDM is not the answer

EPDM has poor resistance to hydrocarbon oils, fuels and greases: a non-polar rubber swells badly in non-polar fluids. Any application involving mineral oil or fuel contact points to nitrile or chloroprene instead. Conversely, EPDM is the standard choice for glycol-based brake fluid, hot water and steam, where nitrile would fail.

Storage

Store bales in a cool, dry place out of direct sunlight. EPDM is stable in storage and does not suffer the crystallisation that affects some other elastomers, but uncured compounds should still be used in rotation since cure behaviour drifts over long periods.

Frequently asked questions

Why does EPDM resist ozone when other rubbers do not?
Because its main chain is saturated. Ozone attacks carbon–carbon double bonds, and EPDM keeps its unsaturation in a small side-chain diene used only as a cure site, leaving nothing in the backbone to attack. Rubbers with unsaturated backbones crack outdoors without antiozonant protection.
Should EPDM be cured with sulphur or peroxide?
Peroxide where heat resistance and compression set matter — a seal that must keep sealing after years under load at temperature. Sulphur where cost and mechanical properties matter more. Peroxide compounds are more expensive and more sensitive to formulation, since many common ingredients interfere with the cure.
What does higher ethylene content give me?
More crystallinity, which means greater green strength, better shape retention during extrusion and the ability to carry very high filler and oil loadings. Lower-ethylene grades are amorphous, stay flexible in the cold and give better compression set.
Can EPDM be used with oil or fuel?
No. EPDM is non-polar and swells badly in hydrocarbon oils, fuels and greases. Those applications need nitrile or chloroprene. EPDM is, however, the standard choice for glycol-based brake fluid, hot water and steam, where nitrile fails.