Pigments and optical additives for plastics, coatings and fibre — opacity, jetness and the brightening that cancels a yellow cast.

Three different ways to change appearance

The materials in this category look related but work by entirely different mechanisms, and confusing them leads to the wrong specification.

Titanium dioxide provides opacity by scattering light. Its refractive index is high enough that a few percent in a polymer or dry film hides the substrate completely, and nothing else achieves this at comparable cost. Rutile grades are specified for plastics and anything outdoors; anatase is brighter but photocatalytically more active and can accelerate degradation of the surrounding polymer or binder.

Carbon black provides colour and tinting strength, and simultaneously acts as the most effective ultraviolet stabiliser available for polyolefins. Particle size drives the trade-off: finer grades give higher jetness and a bluer undertone but disperse harder and raise viscosity.

Optical brighteners provide no covering power at all. They convert invisible ultraviolet into visible blue, cancelling the yellow cast that polymers and recycled content carry, at loadings in the hundredths of a percent.

Dispersion decides the result

With all three, dispersion matters more than loading. Agglomerated titanium dioxide contributes nothing to opacity while showing as specks and raising screen pressure; a well-dispersed 4% is whiter than a poorly dispersed 6%. Agglomerated carbon black leaves unprotected polymer between particles, so the stated percentage does not translate into actual UV protection, and the agglomerates become crack initiation points.

Where dosing accuracy or dispersion is difficult, delivery through a masterbatch is the reliable route.

Matching the grade to the application

Surface treatment is what separates grades that look similar on a specification sheet. Alumina and silica treatments on titanium dioxide improve dispersion and passivate photocatalytic activity; a weathering grade carries heavier treatment and therefore slightly lower TiO₂ content, which is the grade working as intended rather than a quality shortfall.

For optical brighteners, processing temperature decides between OB and OB-1 — OB-1 survives above 350 °C where OB would decompose, while OB disperses more easily at moderate temperatures.

Technical and safety data sheets and samples are available on request. Tell our team the polymer, the process and the appearance target, and we will work back to the grade.