What a plasticiser is chosen for
Every plasticiser softens PVC. What distinguishes them is what happens next: whether the compound stays flexible in the cold, whether the plasticiser is still there after five years at temperature, and what else it contributes to the formulation. Those secondary properties are what grade selection is actually about.
Choosing by service condition
If the part has to stay flexible in the cold, the answer is an aliphatic ester. DOA covers most cold-flexibility requirements economically, and DOS goes further for severe low-temperature service, with lower volatility, at a higher cost. Both are normally used as part of a blend rather than alone, because adipates and sebacates are more volatile than a general-purpose primary.
If the part has to endure heat for years, the answer is a trimellitate. TOTM is the standard for 105 °C cable insulation and long-service flexible PVC, because its larger molecule stays in the compound where a general-purpose plasticiser migrates out and leaves the material hard and cracked.
Plasticisers that do a second job
ESBO is a secondary plasticiser whose real value is chemical: its epoxide rings absorb the hydrogen chloride that drives PVC degradation, which is why calcium-zinc and barium-zinc stabiliser systems work far better with it present. Typical use is 2–5 phr as a co-stabiliser, or up to 25 phr where it also carries part of the softening requirement.
Chlorinated paraffin contributes plasticisation at lower cost while adding chlorine to the flame-retardant system, working alongside antimony trioxide. Chain length matters here for regulatory reasons as much as technical ones: short-chain grades are internationally restricted, and the medium and long chain materials are what is commercially supplied.
How the choice is usually made
Most formulations use a blend. A primary plasticiser carries the bulk of the softening requirement, and secondaries are added to meet specific targets — cold flexibility, heat endurance, flame contribution or stabiliser support. Where a part has to pass both a low-temperature bend test and a heat-ageing weight-loss limit, the ratio is settled by trial against both tests rather than calculated.
Technical and safety data sheets and samples are available on request. Tell our team what the compound has to pass and we will work back to a plasticiser package.