Skip to content

Product category

Flame Retardants

Halogenated and halogen-free flame retardant systems — antimony synergists, mineral hydroxides and multifunctional additives selected by processing temperature and smoke requirements.

Two different approaches to the same problem

Flame retardancy is achieved either in the gas phase or in the condensed phase, and the choice between them is usually made by the specification rather than by the formulator.

Halogenated systems work in the gas phase: a chlorine or bromine source releases halogen radicals that interrupt combustion chemistry, with antimony trioxide as the synergist that makes the mechanism efficient. These systems are effective at low loadings and are economical, but they release corrosive acid gas and dense smoke when they burn.

Mineral systems work physically. Aluminium hydroxide and magnesium hydroxide decompose endothermically, absorbing heat and releasing water vapour that dilutes the flame, leaving an insulating oxide layer behind. No halogen, no acid gas and much less smoke — at the cost of very high loadings.

ATH or MDH: processing temperature decides

The two mineral hydroxides work identically and differ in one number. Aluminium hydroxide begins releasing its water around 200 °C, so any compound processed above that decomposes the filler in the extruder rather than in a fire — producing porosity, surface defects and a product that has already spent its flame retardancy. Magnesium hydroxide is stable to roughly 330 °C.

Polyethylene and EVA compounds generally process below 200 °C and are well served by ATH. Polypropylene, polyamide and engineering polymer compounds are not, and that is where MDH becomes necessary rather than merely preferable.

Where zinc borate fits

Zinc borate is multifunctional rather than primary. It promotes char, forms a glassy barrier layer, suppresses smoke and afterglow, and provides anti-tracking behaviour. In halogenated systems it can replace part of the antimony trioxide. In halogen-free systems it helps the mineral residue sinter into a coherent insulating layer, which can allow a lower total filler loading and recover mechanical properties.

What the loading costs

Mineral systems need 55–65% filler by weight, and no polymer carries that much without losing elongation and tensile strength. Managing this is the real formulating work: base polymers are chosen for filler acceptance — EVA in particular — and surface-treated filler grades with coupling agents recover a meaningful part of the lost properties. Our ready-formulated HFFR compound addresses this directly for cable applications.

Technical and safety data sheets and samples are available on request. Tell our team the polymer, the processing temperature and the test standard, and we will work back to a system.

Need a grade that is not listed?

Our portfolio moves with the market. Describe your specification and we will source or recommend the closest matching material.