Skip to content

HFFR — Halogen-Free Flame Retardant

HFFR compounds are halogen-free flame-retardant materials developed for cables used in buildings, transportation systems and industrial facilities. They help limit flame propagation while reducing smoke and corrosive gas emissions during combustion.

HFFR — Halogen-Free Flame Retardant

At a glance

Category Cable Compounds
Material type Halogen-free flame retardant cable compound (HFFR / LSZH)
Appearance Natural or coloured pellets
Base polymer Typically EVA or polyolefin blend selected for mineral filler acceptance
Flame retardant system Mineral — aluminium hydroxide or magnesium hydroxide, typically 55–65% loading
Halogen content Assessed against EN 60754-1 / IEC 60754-1
Acid gas and conductivity Assessed against EN 60754-2 / IEC 60754-2
Smoke density Assessed against EN 61034-2 (3 m cube test)
Flame propagation Commonly specified against IEC 60332-1 and, for bunched cable, IEC 60332-3
Packaging 25 kg bags, 1,000 kg big bags
Documentation TDS and SDS on request
Supplied from Istanbul, Türkiye

Need this material?

Tell us the application, the specification and the volume you work with. Our team will come back with availability and the documentation you need.

Description

What problem HFFR solves

In an enclosed fire, most casualties are caused by smoke and toxic gas rather than by flame. Halogenated cable materials such as PVC perform well against flame spread, but when they burn they release hydrogen chloride: a dense, acrid smoke that obscures escape routes, is corrosive to people and to equipment, and continues attacking electronics and structural steel long after the fire is out.

Halogen-free flame retardant compounds — also called LSZH, low smoke zero halogen — are formulated so that neither happens. There is no halogen in the formulation to release, and the flame-retardant mechanism itself produces water vapour.

How the mineral system works

Flame retardancy comes from a very high loading of mineral hydroxide, usually aluminium hydroxide or magnesium hydroxide, typically 55 to 65% by weight. When the compound is heated to its decomposition temperature, the filler breaks down endothermically and releases water vapour. That reaction does three things at once: it absorbs heat from the burning surface, the water vapour dilutes the combustible gases in the flame, and the residual oxide forms an insulating ceramic layer over the surface.

The choice between the two fillers is a question of processing temperature. Aluminium hydroxide begins decomposing around 200 °C, so it cannot be used in compounds processed above that. Magnesium hydroxide is stable to roughly 330 °C, which makes it the choice for polypropylene-based and higher-temperature systems, at a higher raw material cost.

Why the base polymer matters so much

A 60% mineral loading is enormous. Most polyolefins become brittle and unprocessable long before that level, which is why HFFR compounds are built on polymers chosen specifically for filler acceptance — usually EVA or a tailored polyolefin blend. The polarity of EVA's vinyl acetate groups lets it wet and hold the mineral surface, so the compound retains enough elongation and tensile strength to survive extrusion, bending and installation.

This is also why HFFR compounds are formulated products rather than simple blends, and why mechanical properties differ noticeably between grades that look similar on a flame specification.

The standards that actually get specified

Four test families typically appear together in a specification. EN 60754-1 measures the halogen acid gas content of the combustion gases. EN 60754-2 measures their pH and conductivity, which is how corrosivity is quantified. EN 61034-2, the three-metre cube test, measures light transmission through the smoke and is what "low smoke" means in practice. IEC 60332-1 assesses flame propagation on a single vertical cable, with IEC 60332-3 covering bunched cables in a vertical tray.

Passing one of these does not imply passing the others — a compound can be halogen-free and still produce substantial smoke — so specifications normally name each test individually.

Where HFFR is required

Typical applications are cable for buildings with high occupancy or restricted escape, rail and metro rolling stock and infrastructure, tunnels, marine and offshore installations, data centres and other equipment-dense environments where corrosive gas would cause severe secondary damage.

Processing and storage

Highly filled compounds are abrasive and raise head pressure; screw and die wear is a real maintenance consideration. Melt temperature must stay comfortably below the filler decomposition temperature, since premature water release causes porosity and surface defects. Store bags sealed and dry: mineral fillers are hygroscopic, and absorbed moisture shows as voids and surface roughness in the extrudate. Condition material to workshop temperature before use.

Frequently asked questions

What does halogen-free actually mean for cable?
That the compound contains no halogenated ingredients, so burning it releases no hydrogen chloride or similar acid gas. It is verified by test rather than by formulation claim — EN 60754-1 measures halogen acid gas content and EN 60754-2 measures the pH and conductivity of the combustion gases, which is how corrosivity is quantified.
Is halogen-free the same as low smoke?
No, and specifications name them separately for that reason. A compound can contain no halogen and still produce substantial smoke. Low smoke performance is measured by EN 61034-2, the three-metre cube test, which assesses light transmission through the smoke produced.
Should the mineral filler be ATH or MDH?
It depends on processing temperature. Aluminium hydroxide starts decomposing around 200 °C and cannot be used above that. Magnesium hydroxide is stable to roughly 330 °C, which makes it necessary for polypropylene-based and higher-temperature compounds, at a higher raw material cost.
Why do HFFR compounds have lower mechanical properties than PVC?
Because of the filler loading. Flame retardancy requires 55–65% mineral by weight, and no polymer carries that much filler without losing elongation and tensile strength. The base polymer is chosen specifically for filler acceptance — usually EVA — which is what keeps the properties usable at all.

Request documentation or a sample

Technical data sheets, safety data sheets and samples are provided on request. Describe your application and we will recommend the closest matching grade.