EVA — Ethylene Vinyl Acetate
EVA is polyethylene with vinyl acetate comonomer built in — the more acetate, the softer, clearer and more adhesive the material becomes.
View detailsProduct category
Thermoplastics and elastomers for compounding and conversion — EVA, POE, TPU, CPE and the synthetic rubbers, selected by the environment the part has to survive.

EVA is polyethylene with vinyl acetate comonomer built in — the more acetate, the softer, clearer and more adhesive the material becomes.
View details
Thermoplastic polyurethane combines rubber-like elasticity with the abrasion resistance of an engineering plastic — and the choice between polyester and polyether backbones decides whether it survives oil or water.
View details
Chlorinated polyethylene is the impact modifier that makes rigid PVC profile survive a cold morning — and because it carries chlorine, it does so without diluting the compound's flame performance.
View details
Chloroprene rubber is the all-rounder: not the best at any single property, but the only common elastomer that is simultaneously respectable against oil, weather, ozone and flame.
View details
EPDM has a fully saturated backbone, which is why it simply does not care about ozone, weather or UV — the properties that make it the standard for anything living outdoors.
View details
Nitrile rubber is the standard answer to oil resistance — and the acrylonitrile percentage is a dial that trades cold flexibility for exactly that.
View details
Polyolefin elastomers are metallocene-made ethylene copolymers that behave like rubber but process like a thermoplastic — the standard way to stop polypropylene from being brittle.
View detailsPolymer selection is rarely about headline mechanical figures. It is about which environment the part has to live in, because that narrows the field faster than anything else — and the trade-offs between the common materials are well understood.
EVA is polyethylene with vinyl acetate comonomer, and almost every property tracks that single variable: more acetate means softer, clearer, more polar and more adhesive. Its polarity is why EVA accepts the very high mineral loadings that halogen-free flame-retardant compounds require.
Polyolefin elastomer behaves like rubber but processes as a thermoplastic, and is the standard impact modifier for polypropylene at 5–25%. Density is the most useful indicator of how a grade will behave.
Thermoplastic polyurethane combines rubber-like elasticity with very high abrasion resistance. The polyester or polyether decision governs service durability: polyester for oil and abrasion, polyether for hydrolysis resistance and cold flexibility.
Chlorinated polyethylene serves as both an impact modifier for rigid PVC at 5–10 phr and as a polymer in its own right for weather- and oil-resistant compounds, with inherent flame resistance from its chlorine.
Three materials cover most elastomer requirements, and the harshest environment decides between them. Nitrile rubber for oil and fuel contact, with acrylonitrile content trading oil resistance against cold flexibility. EPDM for weather, ozone and steam, thanks to its saturated backbone. Chloroprene rubber where oil, weather and flame requirements appear together, which it is uniquely able to satisfy at once.
Start from the most hostile condition in the specification and let it eliminate materials, then check the remaining candidates against the secondary requirements. Where no single polymer satisfies everything, blending or a compound is normally the answer rather than compromising on the critical property.
Technical and safety data sheets and samples are available on request. Describe the service environment and the process, and our team will work back to the polymer.
Our portfolio moves with the market. Describe your specification and we will source or recommend the closest matching material.