NBR — Nitrile Butadiene Rubber
Nitrile rubber is the standard answer to oil resistance — and the acrylonitrile percentage is a dial that trades cold flexibility for exactly that.
- CAS Number: 9003-18-3

At a glance
| Category | Polymers |
|---|---|
| CAS Number | 9003-18-3 |
| Chemical name | Acrylonitrile butadiene rubber (nitrile rubber, NBR) |
| Appearance | Bales or chips |
| Acrylonitrile content | Typically 18–50%; oil resistance rises and cold flexibility falls as it increases |
| Service temperature | Typically −30 °C to +100 °C depending on compound and ACN level |
| Curing | Sulphur or peroxide systems |
| Typical applications | Oil seals, O-rings, fuel hose, gaskets, rollers, oilfield parts |
| Packaging | 25–35 kg bales on pallets |
| Documentation | TDS and SDS on request |
| Supplied from | Istanbul, Türkiye |
Need this material?
Tell us the application, the specification and the volume you work with. Our team will come back with availability and the documentation you need.
Description
What acrylonitrile content controls
Nitrile rubber is a copolymer of acrylonitrile and butadiene, and almost every selection decision comes down to the ratio between them. The polar nitrile groups are what resist oil: the more acrylonitrile in the chain, the less a hydrocarbon oil can swell the rubber.
The same polarity stiffens the chain, so the trade is direct and unavoidable. A low-ACN grade around 18 to 20% stays flexible to about −40 °C but swells noticeably in oil. A high-ACN grade at 45 to 50% resists oil and fuel strongly but becomes stiff and brittle not far below freezing. Medium grades in the 33 to 36% range are the general-purpose compromise and cover the majority of seal and gasket work.
Choosing a grade
The practical method is to start from the harsher of the two requirements. If the part sees aggressive fuel or high-aromatic oil, specify the ACN content that controls swell and then check whether the low-temperature requirement can still be met — often with the help of a plasticiser. If low-temperature sealing is critical, start from the ACN that meets it and verify the swell is tolerable.
Where neither can be compromised, hydrogenated nitrile rubber (HNBR) is the usual next step, offering better heat and ozone resistance at a significantly higher cost.
What NBR does not do well
Nitrile rubber has poor resistance to weather, ozone and ultraviolet light. Its butadiene segments carry unsaturation that ozone attacks, and an unprotected NBR part exposed outdoors will crack. Antiozonants and waxes help, and blending with PVC improves weather and ozone resistance markedly — a common approach for hose covers and cable jackets.
It is also unsuitable for polar fluids: brake fluid, ketones and strong acids attack it. And its heat resistance has limits, with continuous service generally capped around 100 °C.
Compounding and curing
NBR cures with sulphur systems or with peroxide. Peroxide curing gives better compression set and heat resistance, which matters for seals held under load at temperature; sulphur curing gives better tensile and tear properties and is more economical. Carbon black is the standard reinforcing filler, with grade and loading setting hardness and modulus.
Storage
Store bales in a cool, dry place out of direct sunlight and away from ozone sources such as electric motors and arc equipment. Keep stock rotated: uncured nitrile compound stiffens over time and its processing behaviour drifts.
Frequently asked questions
What acrylonitrile content should I specify?
Why does NBR crack when used outdoors?
Should NBR be cured with sulphur or peroxide?
Is NBR suitable for brake fluid or ketones?
Request documentation or a sample
Technical data sheets, safety data sheets and samples are provided on request. Describe your application and we will recommend the closest matching grade.