XLPE NATURAL — Crosslinkable Polyethylene

Silane-grafted XLPE compound with catalyst masterbatch for insulation of 0.6/1 kV low-voltage power cables

XLPE NATURAL — Crosslinkable Polyethylene

At a glance

Category Cable Compounds
Material type Silane-grafted crosslinkable polyethylene insulation compound, supplied with catalyst masterbatch
Appearance Natural pellets; catalyst masterbatch supplied separately
Crosslinking method Moisture cure (silane / Sioplas or Monosil route)
Rated voltage Suitable for 0.6/1 kV low-voltage power cable insulation
Continuous conductor temperature Typically rated 90 °C once crosslinked
Short-circuit rating Typically 250 °C for the standard short-circuit duration
Mixing ratio Base compound to catalyst masterbatch as stated on the technical data sheet; typically 95:5
Packaging 25 kg moisture-barrier bags
Documentation TDS and SDS on request
Supplied from Istanbul, Türkiye

Need this material?

Tell us the application, the specification and the volume you work with. Our team will come back with availability and the documentation you need.

Description

What crosslinking achieves

Ordinary polyethylene softens and eventually flows as it approaches its melting point, which caps the temperature at which a cable can safely operate. Crosslinking ties the polymer chains together with permanent chemical bonds, so the material can no longer flow. The result keeps the excellent dielectric properties of polyethylene but adds form stability at temperature.

In cable terms the gain is concrete: a crosslinked insulation is typically rated for 90 °C continuous conductor temperature against 70 °C for thermoplastic PVC or PE, and withstands around 250 °C during a short circuit. For the cable designer that means more current through the same conductor cross-section, which is usually the whole reason for specifying XLPE.

How silane crosslinking works

Silane groups are grafted onto the polyethylene chain. After extrusion, when the insulated core is exposed to moisture, those groups hydrolyse and condense with each other to form permanent siloxane bridges between chains. A catalyst masterbatch, blended with the base compound at the ratio given on the data sheet, drives that reaction at a practical rate.

The important consequence is that crosslinking happens after the cable is made, not in the extruder. The compound extrudes as a conventional thermoplastic — no special head, no curing tube, no peroxide — and is then cured in a warm water bath or steam, or more slowly in ambient humidity. This is why silane crosslinking is the standard route for low-voltage cable: the equipment cost is a fraction of the peroxide-cured route used for medium and high voltage.

Handling the moisture sensitivity

The same chemistry that makes the system convenient makes it demanding in storage. Moisture reaching the compound before extrusion begins crosslinking prematurely, producing gels and surface defects in the insulation and, in severe cases, material that cannot be extruded at all. Bags are supplied with a moisture barrier and must be kept sealed until use, opened material consumed promptly, and the catalyst masterbatch handled with the same care.

Mixing ratio accuracy matters too. Too little catalyst leaves the cure incomplete, so the insulation never reaches its rated properties; too much can cause premature crosslinking during extrusion.

Verifying the cure

Crosslinking is not visible, so it is verified by test — most commonly a hot-set test, in which a sample is loaded at elevated temperature and its elongation measured. A properly cured sample extends by a limited amount and recovers; an undercured one extends excessively or fails. Cure time depends on wall thickness, water temperature and ambient humidity, and should be established for the specific construction rather than assumed.

Storage

Store in sealed moisture-barrier bags in a cool, dry place, well away from water and steam sources. Observe the shelf life stated on the data sheet: even sealed, silane-grafted compound has a finite storage life. Condition bags to workshop temperature before opening so that condensation does not form on cold pellets.

Frequently asked questions

Why does XLPE allow a higher cable rating than PE or PVC?
Because crosslinking stops the polymer flowing at temperature. A crosslinked insulation is typically rated 90 °C continuous against 70 °C for thermoplastic PE or PVC, and withstands around 250 °C in a short circuit. That allows more current through the same conductor cross-section.
What does the catalyst masterbatch do?
It drives the moisture-cure reaction at a practical rate. The silane groups grafted onto the polymer hydrolyse and condense into siloxane bridges when exposed to water, and the catalyst makes that happen in hours rather than indefinitely. Mixing ratio accuracy matters: too little leaves the cure incomplete, too much risks crosslinking in the extruder.
Why must silane XLPE compound be kept sealed?
Because moisture starts the crosslinking reaction. Compound that has picked up water before extrusion forms gels and surface defects in the insulation and in bad cases becomes unextrudable. Bags carry a moisture barrier, should stay sealed until use, and opened material should be consumed promptly.
How is the degree of crosslinking checked?
Usually by hot-set test: a sample is loaded at elevated temperature and its elongation measured. A properly cured sample extends by a limited amount and recovers, while an undercured one extends excessively or fails. Cure time depends on wall thickness, water temperature and humidity, so it should be established per construction.